A335 P5 Speċifikazzjoni tal-Pajp tal-Azzar Liga
| Firxa Daqs | 1/8" –42" |
| Skedi | 20, 30, 40, Standard (STD), Extra Heavy (XH), 80, 100, 120, 140, 160, XXH & itqal |
| Standard | ASTM A335, ASTM A213 |
| Grad |
ASTM A335 P1, P2, P5, P9, P11, P12, P22, P23, P91, P92, ASTM A213 T2, T5, T5b, T5c, T9, T11, T12, T22, T23, T91, T92 |
Kompożizzjoni Kimika % Tal-Pajp tal-Azzar Liga A335 P5
|
Kompożizzjonijiet |
Data |
|
Deżinjazzjoni UNS |
K41545 |
|
Karbonju (mass.) |
0.15 |
|
Manganiż |
0.30-0.60 |
|
Fosfru (mass.) |
0.025 |
|
Silikon (mass.) |
0.50 |
|
Kromju |
4.00-6.00 |
|
Molibdenu |
0.45-0.65 |
|
Elementi Oħra |
… |

Proprjetajiet Mekkaniċi Ta 'A335 P5 Alloy Steel Pipe
|
Proprjetajiet |
Data |
|
Saħħa tat-tensjoni, min, (MPa) |
415 Mpa |
|
Qawwa ta' rendiment, min, (MPa) |
205 Mpa |
|
Titwil, min, (%), L/T |
30/20 |
Pajp ASTM A335 P5 huwa komunement użat f'servizzi ta 'temperatura għolja bħal bojlers, skambjaturi tas-sħana, sistemi ta' pajpijiet ta 'pressjoni għolja, u applikazzjonijiet simili. Jistgħu jintużaw biex jittrasportaw fwar, likwidi u gassijiet b'temperatura għolja, eċċ.
Il-kumpanija tagħna għandha vantaġġi kompetittivi sinifikanti fl-industrija. Aħna nispikkaw għall-prodotti tagħna tal-pajpijiet tal-azzar ta 'kwalità għolja u s-soluzzjonijiet professjonali, b'teknoloġija ta' produzzjoni avvanzata u esperjenza rikka. Is-saħħa tagħna tinsab mhux biss fil-proċessi ta 'produzzjoni awtomatizzati ħafna tagħna, iżda wkoll fl-impenn tagħna li nipprovdu servizz tal-konsumatur eċċellenti u twassil f'waqtu biex nissodisfaw il-ħtiġijiet tal-klijenti tagħna.