Feb 18, 2024

  • GB 5310-2008 tubi tal-bojler bi pressjoni għolja huma maqsuma fi tliet kategoriji skond il-materjal

1. Materjali tat-tubi tal-bojler ta 'pressjoni għolja ta' l-azzar strutturali tal-karbonju ta 'kwalità għolja huma 20G, 20MnG, u 25MnG;

2. Materjali tat-tubi tal-bojler bi pressjoni għolja tal-azzar strutturali liga huma 15MoG, 20MoG, 12CrMoG, 15CrMoG, 12Cr2MoG, 12Cr1MoVG, 12Cr2MoWVTiB, 07Cr2MoW2VNbB, 12Cr2MoW2VNbB, 12Cr2MoW2VNbB, 12Cr2MoW2VNbB, 12Cr2MoW2VNbB, 12Cr2MoW2VNbB, 12Cr2MoW2VNbB, 12Cr2MoW2VNbB, 12Cr2MoW2VNbB, 12Cr2MoW2VNbB, 12Cr2MoW2VNbB NbN, 10Cr9MoW2VNbBN, 10Cr11MoW2VNb Cu1BN, 10Cr9Mo1W1VNbBN;
3. Materjali tat-tubi tal-bojler ta 'pressjoni għolja ta' l-azzar li ma jsaddadx (reżistenti għas-sħana) huma 07Cr19Ni10, 10Cr18Ni9NbCu3BN, 07Cr25Ni21NbN, 07Cr19Ni11Ti, 07Cr18Ni11Nb, 08Cr18Ni11Nb, 08Cr18GNi1111

carbon structural boiler pipe

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

  • GB 3087-2008 materjal tat-tubu tal-bojler bi pressjoni baxxa u medja: 10#, 20#

  • GB/T 20409-2006 Materjali tat-tubi tal-bojler tal-ħajt intern bi pressjoni għolja: 20G, 20MnG, 25MnG, 12CrMoG, 15CrMoG

low pressure boiler tube